3D printed superalloy cut down carbon emissions: Sandia

Posted on 2023-03-212023-03-21 by coilss.com

Researchers from Sandia National Laboratories have shown that a new 3D printed superalloy could help power plants generate more electricity while producing less carbon.
Sandia scientists collaborated with researchers at Ames National Laboratory, Iowa State University, and Bruker Corp. on the project.
The institution said that the experiments showed that the new superalloy – made up of 42% aluminium, 25% titanium, 13% niobium, 8% zirconium, 8% molybdenum, and 4% tantalum – was stronger at 800°C than many other high-performance alloys, including those currently used in turbine parts. The team also said it was still stronger when it was brought back down to room temperature.
According to Sandia National Laboratories, the findings could have broad impacts across the energy sector as well as the aerospace and automotive industries, and hints at a new class of similar alloys waiting to be discovered. Sandia says that the superalloy development represents a ‘fundamental shift’ in alloy development as no single material makes up more than half the material.
Sandia states that the research team is interested in exploring whether advanced computer modelling techniques could help researchers discover more members of what could be a new class of high-performance additive manufacturing-forward superalloys.

Previous articleAerolloy Technologies signs MoU with Dassault Aviation
Next articleRuby Sharma joins the ATI Board of Directors

Stainless Steel World is part of The KCI Media Group, a group of companies focused on building and sustaining global communities in the flow control industries. We publish news on a daily basis and connect business-to-business professionals through our online communities, publications, conferences and exhibitions.

Recent Posts

  • Systematic fraud in steel imports?
  • Indonesia running out of low-grade nickel ore
  • What is Electropolished Tubing? Benefits of Electropolishing
  • EU steel demand expected to rise again
  • EOGEPL invest in Microbial eCBM to boost CBM production

Recent Comments

No comments to show.

Category

  • Stainless Steel
©2023 Welcome to Ly Steel ! | Built using WordPress and Responsive Blogily theme by Superb